Corrosive influence - The dangers of galvanic corrosion for pipelines

Geir otto Amundsen • March 10, 2025

Norway’s key processing plants used for the transportation and processing of gas and condensate/light oil has successfully sealed previously sustained leaks. Located in Kårstø, Norway it is one of the largest of its kind in Europe, it found itself plagued with leaks in its condensed steam piping system. After trying various gasket sealing solutions to stop the leaking flanges, the leaks were completely eliminated through the utilization of the DeltaV-Seal. The DeltaV-Seal offers a gas-tight, metal-to-metal solution that is capable of operating in extreme temperatures without developing deposits on the flanges.

Operating conditions expose gaskets to excessive strain, normally leaving deposits on the flange.

Leakage in piping installations constitute a major challenge at processing plants. High pressure steam, various chemical components, and severe temperature fluctuations put strain on the joint flanges of gasket seals. Even small leaks may cause major problems, as well as power loss and unwanted strain on the pipe system. Leaks may also cause pollution problems detrimental to the plant itself, the working environment, and the surrounding environment.


The plant experienced leakage over an extended period of time, despite several attempts which were made to seal the flange using various, competing sealing solutions. However, Tvedestrand based Pipeotech offered to deliver its new and patented DeltaV-Seal seal system to the 18-inch flange, free of charge, enabling the plant operator to test the quality.


The DeltaV-Seal was delivered in 316L material, which matched the flange material. Manufacturing the DeltaV-Seal out of the same material as the flange prevents galvanic corrosion from developing, further protecting the flange’s integrity.


Attending the installation of the DeltaV-Seal at the plant was Pipeotech Sales Manager Erlend Berntsen and Chief Technical Officer Frode H. Larssen. Mr Berntsen explained how the core principle of DeltaV-Seal is to make the seal from the same metal as the flange itself, in addition to integrating elevated rings that adapt to the shape of the flange when bolted together.

– Our sealing system proved effective both against gas and liquid leaks, as well as chemical components prone to corroding other sealing solutions. The DeltaV-Seal withstands large temperature variations and does not cause depositing, which is often a challenge when replacing gaskets.

Erlend Berntsen, Direct Sales Manager, Pipeotech AS

When opening the flange to install the DeltaV-Seal, the flange required a time-consuming process of being cleaned of packaging residue and old sealants. The leaking flange was located several meters up on the rig and a mobile crane was required in order to complete the installation process. The process of removing and cleaning the previously failed seal required four mechanics and a security guard to work an entire day to complete before the new seal could be inserted.

The flange the leak was located at a flange several meters up on the rig and a mobile crane was required in order to complete the installation process.

After installation of the DeltaV-Seal was completed a test report confirmed the flange became 'gas-tight' and all leakage was eliminated after the old seal was replaced.


Another advantage of the DeltaV-Seals metal to metal design is that it does not require post-tightening or re-torquing of bolts at any time during its operational life cycle. In addition to the successful remedy of the previously persistent leak, thanks to the design of the DeltaV-Seal and ease of installation, the cost of the process was below the estimated cost.

– We are now eager to see if the success of this test will pave the way for the use of our solution in the rest of the plant, as well as in other company installations with leakage issues caused by pressure, vibrations, or temperature fluctuations.

Erlend Berntsen, Direct Sales Manger, Pipeotech AS

May 14, 2025
We are excited to announce our participation in the 15th European Pressure Equipment Symposium, taking place on July 1–2, 2025 , in Fürstenfeldbruck , near Munich. Our team will be on-site as exhibitors, and we warmly invite you to visit our booth and connect with our colleagues Andrew Patrick, Jan Oredsson and Erlend Berntsen. This event offers a great opportunity to exchange ideas, learn about the latest developments in the field, and explore how we can support your goals. To learn more about the event, please visit: www.tuvsud.com/akademie/europaeische-druckgeraetetage We look forward to welcoming you in Fürstenfeldbruck!
By James Knights • March 17, 2025
Fertilizers are critical to enable the growing global population to be fed. Ongoing increases in energy prices, particularly methane, have made the cost of manufacturing nitrogen and ammonia-based fertilizers particularly high. Anything a manufacturer can do to reduce costs, reduce NOX emissions, and increase reliability has a positive global impact, ensuring a secure and long-term food supply while at the same time increasing reliability and reducing maintenance costs.
By James Knights • March 17, 2025
Ammonium Nitrate is a challenging chemical to seal, in addition to being extremely hazardous. When Ammonium Nitrate emissions escape from bolted flange joints it crystalizes. These crystals of Ammonium Nitrate are a safety hazard and undesirable. Further to this the Ammonium Nitrate crystals can form inside the pipe, reducing flow and productivity. To remove the crystals of Ammonium Nitrate inside the piping, steam cleaning is utilized. This increases the degradation of legacy semi-metallic gaskets leading to an increased leakage rate, which results in more emissions, more crystals, and a cycle of avoidable costly maintenance.
By James Knights • March 17, 2025
A leading chemical manufacturer sought a superior gasket to replace the current semi-metallic gasket utilized throughout this specific vacuum system. For this system it is crucial to prevent oxygen from entering the vacuum system as it would cause oxidation of the piping contents and compromise the entire batch of chemicals, leading to it being wasted. The DeltaV-Seal, known for its tightness and durability, prevents oxygen from entering the system through the bolted flange joints. This ensures that the product passed through the piping system is not contaminated by oxygen from the bolted flange joints, providing a superior quality end product.
By James Nights • March 14, 2025
The United States Clean Air Act (CAA) is the comprehensive federal law regulating emissions from stationary and mobile sources.  Among other things the CAA authorises the United States Environment Protection Agency (EPA) to establish National Ambient Air Quality Standards (NAAQS) to protect the public health and public welfare as well as regulate emissions of hazardous air pollutants. The DeltaV-Seal effectively removes fugitive emissions fugitive emissions from connections, this case study details how.
By James Knights • March 14, 2025
Imagine a future where in extreme environments it is possible to model and simulate a gaskets performance and know the lifetime of a bolted flange joint, sealed with a DeltaV-Seal. Pipeotech's Engineering and Technical team have been working to make the modelling and simulation of a gasket a possibility. Being able to simulate the performance of a bolted flange joint, and provide a defined lifetime has huge financial benefit to industry, maximising the time between turnarounds, extracting maximum value from their assets.
More Posts